The optical properties of glasses irradiated by high-power, 810 nm femtosecond laser have been studied. Laser-induced processes occurred at irradiation well below the threshold for laser-induced damage. The visible absorption spectra of the original and irradiated glass were measured and darkening lines were found in the irradiated region. According to absorption spectra, the absorption of glass was increased greatly after irradiation by femtosecond laser. The absorption of the irradiated glass decreased along with time and reached stabilization in about 90 minutes. The laser-induced darkening in the glass disappeared when the glass was heat-treated under 200 degrees Celsius for a few minutes. It was considered that darkening was induced by color-center formation because of glass matrix photoionization and the consequent trapping of electrons and holes by intrinsic or impurity defect of the glass. This process is expected to become a useful method used to fabricate optical memory with both an ultra-high storage density and an ultra-high recording and readout speed.
© (2001) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Xiongwei Jiang, Congshan Zhu, and Fuxi Gan "Femtosecond-laser-induced recording in glass", Proc. SPIE 4085, Fifth International Symposium on Optical Storage (ISOS 2000), (7 February 2001); https://doi.org/10.1117/12.416845
Lens.org Logo
CITATIONS
Cited by 2 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Glasses

Absorption

Femtosecond phenomena

Optical storage

Electrons

Silica

Laser damage threshold

Back to Top